The ring test (RT) was proposed by Hobbs ( 1965 ) to improve the indirect tensile test (Brazilian test, BT), consisting in performing the Brazilian test on a sample with a hole inside it. The ring test was not recognized as a valid laboratory test because the available analytical solution gave incoherent results (Jaeger and Hoskins 1966 ; Mellor and Hawkes 1971 ); in the case of a specimen with a tiny hole, the tensile strength would be six times greater than that obtained with the Brazilian test. Furthermore, the values of the tensile strength applying the analytical solution are very dependent on the sample geometry, changing in function of its diameters and thickness.