Precipitated lignin from black liquor, waste stream of empty fruit bunch (EFB) delignification, was pyrolyzed to yield porous carbon material for H 2 storage. Physisorption capacity was governed mainly by pore volume, while trace metals detected on carbon surface increased total H 2 uptake through chemisorption. Pyrolyzed lignin releases physisorbed H 2 upon mild heating. However, hydrogen bound to metal sites generally requires higher temperatures for desorption during redox cycling. Pyrolyzed lignin obtained at 700°C exhibited the highest porosity with specific surface area (SSA) 416.1 m²/g and thermal-conductivity-detector (TCD) desorption peak area 0.072 a.u. Morphological (SEM-EDS) and elemental (ICP-OES) analyses confirmed the presence of metals on pyrolyzed lignin surface. Density functional theory (DFT) calculation supported this behaviour by identifying the corresponding adsorption energies ( 𝐸 𝑎 𝑑 𝑠 ) of metal oxide. Physisorption accounted 73.7% of total H 2 storage capacity, while the remaining 26.3% was attributed to chemisorption. Low-temperature H 2 adsorption-desorption cycling, up to 85°C, confirmed physisorption-dominated release, consistent with low 𝐸 𝑎 𝑑 𝑠 values of DFT calculation for CaO and MgO. Repeated cycling showed 11.3% decrease in H 2 storage after the second cycle.
No takes yet. Share an insight, caveat, or question.
Prasetyo et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: