The material efficiency of electrophoretic deposition of a fluorene-based conjugated polymer, poly[(9,9-dioctyl-2,7-divinylenefluorenylene)-alt-{2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylene}] (PDOF-MEHPV), from suspensions with a mixture of acetonitrile and toluene as dispersant is studied. It has been found that the recovery rate of the electrophoretic deposition from a suspension containing 90% of the poor solvent acetonitrile reaches 98%. Although the recovery rate decreases with decreasing acetonitrile content, almost 70% of the polymer can be deposited on the substrates from the suspension containing equivalent volumes of the good and poor solvents by electrophoretic deposition, from which smooth and transparent films suitable for electronic devices are obtained.