This is the authors' abstract. We don't add key points for this paper.
The modified oxalate precursor method was used for the preparation of nanocrystalline CoFe2O4. Structural investigations of as-produced powders performed by means of high-resolution transmission electron microscopy and X-ray diffraction revealed an average particle size of 8 nm. The nanocrystallites are pure CoFe2O4 and present a well crystallized spinel structure with lattice constant of 8.3583 Å. The particles are superparamagnetic exhibiting a blocking temperature around room temperature. The magnetization and the coercive field values obtained at 9 T are 56.8 emu · g−1 and 17.0 kOe (at 4.2 K), respectively. The crystalline anisotropy determined from the coercive field as a function of temperature is 8.0 × 105 J · m−3, which is much higher than that of bulk materials.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Turtelli et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: