Catalytic methane decomposition (CMD) is a promising route for the co-production of CO x -free H 2 and value-added carbon, but its practical application is limited by catalyst deactivation caused by carbon deposition and Ni sintering. In this work, Ni catalysts supported on silica materials with different pore architectures, namely fibrous KCC-1, bimodal porous BPS-5, and channel-type MCM-41 and SBA-15, were systematically compared to clarify the role of support structure in Ni dispersion, carbon deposition, and CMD stability. Among them, Ni(30)/KCC-1 showed the best overall performance, reaching 81.3% CH 4 conversion at 800 °C and maintaining >50% conversion for more than 180 min at 600 °C. The three-dimensional radially fibrous network of KCC-1 favored highly dispersed Ni species, alleviated pore blockage, and promoted the formation of highly graphitized multi-walled carbon nanotubes (I D /I G = 0.88). In contrast, MCM-41 and SBA-15 tended to form larger surface Ni particles and deactivated more rapidly, while BPS-5 only partly relieved diffusion limitations. Kinetic analysis over Ni(30)/KCC-1 gave an apparent reaction order of 1.29 and an apparent activation energy of 47.65 kJ mol −1 , indicating high intrinsic CMD activity. These results demonstrate the structural superiority of KCC-1 as a Ni support and provide guidance for designing durable catalysts for low-carbon hydrogen production with simultaneous carbon nanomaterial valorization.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: