The microstructures, tensile properties and fracture mechanisms of the welded joints of Gd-containing GH3535 superalloy were investigated systematically in this study. Using the low-cost, high-efficiency Keyhole Tungsten Inert Gas (K-TIG) welding technology, the 5 mm-thick alloy plates were successfully welded, which is currently the highest thickness record for the autogenous welding of Gd-containing superalloy. After welding, the granular Ni 5 Gd phase particles in base metal (BM) transform into lamellar γ/Ni 5 Gd eutectic phases in the heat-affected zone (HAZ) by local liquation and re-solidification, while the divorced γ/Ni 5 Gd eutectic phases were formed in the weld metal (WM). The size of Ni 5 Gd phases in WM is smaller than that in BM and HAZ, but their connectivity is the highest. The room-temperature tensile tests show that the welding joints possess a slightly higher yield strength and lower elongation and ultimate tensile strength as compared with the BM samples. Based on the fracture surface observations, all failures of welding joints occurred at the WM, and the cracks are related to divorced γ/Ni 5 Gd eutectic phases. Combining in situ scanning electron microscopy tensile tests and other multiscale characterization techniques, the deformation and fracture mechanisms of welding joints of Gd-containing have been elaborated. In this study, the critical role of divorced γ/Ni 5 Gd eutectic phases in the fracture process of welded joints of Gd-containing superalloy has been clarified, which can guide for optimization of welding parameters and joint design to improve joint performance.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wu et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: