Metal-halide perovskite solar cells (PSCs) achieve high power-conversion efficiencies but remain susceptible to photo-induced degradation caused by mobile ions and phase segregation. Here, we investigate positional isomers of pyridine-carboxylic acid, namely pyridine-2-carboxylic acid (2-PC) and pyridine-4-carboxylic acid (4-PC), as anti-solvent additives to clarify how functional-group orientation governs defect passivation and photo-induced degradation. Both additives improve film morphology and reduce trap density; however, 4-PC, in which the carboxyl group is positioned opposite the pyridine nitrogen, provides markedly stronger passivation by virtue of its more favorable passivation geometry. As a result, 4-PC suppresses light-induced photoluminescence red shift, reduces trap density by approximately 27%, and enables unencapsulated devices to retain over 88% of their initial efficiency after 1000 h. Spectroscopic and transient analyses further indicate that 4-PC simultaneously passivates Pb-related defects and halide vacancies, thereby suppressing ion migration and halide phase segregation under operating conditions. These findings establish positional-isomer engineering as a practical molecular design principle for developing simple yet effective anti-solvent additives toward improved photo-induced phase stability in perovskite photovoltaics.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Lee et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: