This paper presents the preliminary findings of a laboratory study in which the electrochemical behavior of hot-dip galvanized 5% Al–Zn and 55% Al–Zn coatings has been investigated in saturated Ca(OH)2 solution. Experimental results show that, as compared with pure zinc galvanized coating, these two Al-containing coatings have more negative open-circuit potentials (OCPs) and greater passive current densities, yet smaller passive film resistance (Rpf). Therefore, they might have greater corrosion rates. Electrochemical impedance spectroscopy (EIS) displays two maximum phase lags that correspond to two capacitance elements in the equivalent circuit, including double-layer capacitance (Cdl) and passive-film capacitance (Cpf), respectively. After 48 h of immersion in saturated Ca(OH)2 solution, the specimen surfaces are covered with flakes of corrosion products and the coating thicknesses are greatly reduced.
No takes yet. Share an insight, caveat, or question.
Cheng et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: