Answers are grounded in this paper and cite their sources.
Residual old mortar weakens recycled fine aggregate (RFA) and its interface with new paste. This study examined Na 2 CO 3 pre-wetting as a means of storing releasable carbonate in RFA for subsequent aggregate mineralization and matrix modification. RFA was pre-wetted for 3 h with 0-12 wt.% solutions, and direct-addition controls at matched nominal dosages were included. Background-corrected carbonate-equivalent release in deionized water increased with solution concentration. After 28 d in Ca-rich simulated pore solution, the RFA crushing value decreased by up to 16.9% relative to the water-prewetted reference. Compared with direct addition, RFA pre-wetting moderated stiffening, increased heat release between 24 and 72 h, and produced higher 28 d strengths. The paired 72 h cumulative heats nevertheless differed by no more than 3.6%. The 3-6 wt.% mixtures also exhibited higher apparent NMR hydration and silicate chain-length indices than C0. Mortar strength increased up to 6 wt.% and declined at higher concentrations. Relative to C0, C6 exhibited a 50.5% lower near-RFA low-gray area fraction, a 23.8% higher near-RFA indentation modulus, and a 37.8% higher 28 d compressive strength. The approximate defect-enriched width decreased from 55 to 35 μm. Further increasing the concentration to 12 wt.% reduced later heat release and strength despite improved RFA crushing resistance in the simulated environment. These results support a dual-region strengthening interpretation involving aggregate-side mineralization and near-RFA matrix modification, with 6 wt.% as the best tested pre-wetting solution concentration.
No takes yet. Share an insight, caveat, or question.
Qiu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: