Answers are grounded in this paper and cite their sources.
The compositional dependence of phase-formation behavior in fluorite-type ferroelectric films of the binary HfO 2 –ZrO 2 system was systematically evaluated while considering the size effect associated with film thickness. The crystalline phase of the chemical solution deposition-derived films (1– x ) HfO 2 – x ZrO 2 films ( x = 0–1.00) generally exhibited a transition from the monoclinic fluorite ( m -phase) to orthorhombic and/or tetragonal phases ( o -/ t -phase) with increasing the ZrO 2 content. However, the phase boundary between m -phase and o -/ t -phases shifted toward the ZrO 2 -rich region as the film thickness decreased. The composition exhibiting enhanced ferroelectricity also shifted toward the ZrO 2 -rich side, coincident with the phase boundary: the 40 nm-thick films showed the maximum remnant polarization at x = 0.75, which is noticeably different from the commonly reported optimum composition of x = 0.50 (i.e. Hf 0.5 Zr 0.5 O 2 ) for ultrathin (∼9 nm) films.
No takes yet. Share an insight, caveat, or question.
Uchida et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: