Answers are grounded in this paper and cite their sources.
Several methods of drying cement paste prior to determining its physical properties, for example pore size distributions, are critically studied. Phase-pure preparations of ettringite and calcium monosulfoaluminate are used as sensitive indicators of damage. Oven drying at 105°C and drying over strong desiccants, for example MgClO4, is damaging. D-drying for 2–3 h is recommended as a robust but relatively non-damaging treatment. D-drying reduces the water content of ettringite to ∼30 H2O per formula unit, but removal of its zeolitic water, ∼1·7 H2O, does not degrade the structure. Monosulfoaluminate, AFm, is reduced from 12 to 10 H2O with shrinkage of its basal spacing from ∼9·0 to ∼8·2 Å. However, D-drying of pastes from commercial calcium sulfoaluminate rich in AFm usually gives mixtures of the ∼9·0 and ∼8·2 Å phases.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: