Multi-material design shifts the technological bottleneck from the components to the joining operation. In pin joining, metallic pin structures are formed and subsequently mechanically interlocked with a joining partner, enabling the joining of dissimilar materials without auxiliary elements. The in-situ pin caulking joining strategy combines hole formation, insertion and undercut generation in a single stroke, allowing the pin to act both as a forming element and as a load-carrying one, while the geometry after joining, rather than the extruded geometry, defines the interlock. A self-piercing pin (SP-Pin), whose thin walls are spread during the joining stroke, was compared with a solid cylindrical reference pin upset over its full cross-section. Both were joined to a unidirectional glass fibre/polypropylene laminate in four array configurations at constant pin spacing. Spreading the thin walls required less joining force than upsetting the full cross-section, without reducing the undercut. The normal load capacity of the SP-Pin was largely independent of the arrangement. That of the reference pin differed by a factor of 1.58 between the two-pin arrays. This indicates that the normal load capacity is governed mainly by the pin geometry for the SP-Pin and more strongly by the surrounding laminate for the reference pin. In the arrays, the SP-Pin largely maintained its shear force per unit joining force, unlike the reference pin. Despite a 25.0% lower joining force, the 2 × 2 SP-Pin joint carried 1.44 times the shear force and 2.87 times the normal force of the reference joint.
No takes yet. Share an insight, caveat, or question.
Gavelek et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: