Answers are grounded in this paper and cite their sources.
: High-strength AA7075 remains difficult to process by laser powder bed fusion because its broad solidification interval, high thermal conductivity, and evaporation of volatile Zn and Mg promote lack-of-fusion defects, keyhole porosity, and solidification cracking. In this study, TiB 2 nanoparticles were incorporated into gas-atomized AA7075 powder to improve melt-pool stability, refine the solidification structure, and enhance mechanical performance. A Taguchi L9 design was employed to investigate the combined effects of laser power, scan speed, hatch spacing, and TiB 2 content over ranges of 200 to 250 W, 500 to 800 mm s -1 , 70 to 100 μm, and 0.5 to 1.5 wt.%, respectively. Relative density, porosity, lack-of-fusion fraction, keyhole-pore fraction, crack density, maximum crack length, melt-pool geometry, and Vickers microhardness were evaluated to establish the processing window. Three distinct processing regimes were identified. Insufficient energy input produced severe lack-of-fusion defects, as observed in Run 3, which exhibited a relative density of 93.12%, a total porosity of 6.88%, and a LoF fraction of 6.55%. Excessive thermal input promoted unstable keyhole formation and cracking, with Run 8 showing a keyhole-pore fraction of 2.53%, a crack density of 0.68 mm mm -2 , and a maximum crack length of 195.2 μm. Run 9 provided the most favorable overall consolidation response, achieving a relative density of 99.52%, total porosity of 0.48%, crack density of 0.14 mm mm -2 , maximum crack length of 52 μm, and keyhole porosity of 0.26%. Tensile specimens were fabricated in a second build using the Run 9 laser-processing parameters, with TiB 2 content varied from 0.5 to 1.0 wt.% to assess the influence of the reinforcement level under the selected processing conditions. The optimized tensile condition exhibited an ultimate tensile strength of 518 ± 9 MPa, a yield strength of 432 ± 8 MPa, and an elongation of 16.2 ± 0.6%. The maximum measured microhardness within the Taguchi matrix was 158.7 HV. The observed microstructures were consistent with TiB 2 -assisted heterogeneous nucleation, cellular refinement, interruption of continuous epitaxial growth, and reduced crack continuity; these mechanisms are interpreted from the available microscopy and require matched-control quantitative EBSD and TEM confirmation. X-ray diffraction showed retention of the α-Al matrix and TiB 2 phase with no additional crystalline reaction products detected within the XRD detection limit. Overall, the results demonstrate that the processability and mechanical performance of LPBF-fabricated AA7075 cannot be optimized by energy input or reinforcement content alone. Simultaneous control of laser parameters, melt-pool stability, defect evolution, and TiB 2 dispersion is required to produce dense, crack-resistant components with a favorable strength-ductility balance.
No takes yet. Share an insight, caveat, or question.
Sabry et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: