Dynamic behavior of arc bubbles strongly affects arc stability and weld quality in underwater wet welding. Most existing research concentrates on the overall welding process, whereas the initial arc bubble formation at arc ignition remains understudied. In this work, synchronized high-speed imaging and electrical signal acquisition were used to investigate how contact tip-to-work distance (CTWD), wire feed speed and welding voltage affect bubble features and arc stability during arc ignition. Box-Behnken response surface methodology was applied to quantify the effects of the three parameters on maximum bubble radius and bubble lifetime. Arc bubbles show distinct morphologies in growth and collapse stages: horizontally elongated ellipsoids while growing and vertically stretched approximate cones during collapse. Significant interaction exists among CTWD (16 mm), wire feed speed (5 m/min) and welding voltage (31 V), jointly optimizing bubble radius and duration. At the arc initiation stage, reduced maximum bubble radius lowers current variation and unstable arc occurrence. Smaller initial bubbles also mitigate fluctuations of instantaneous heat input, reduce weld pores and macroscopic defects, modify microstructure and improve weld appearance. This work offers new understanding of arc bubble evolution and arc stability during arc ignition of underwater wet welding.
No takes yet. Share an insight, caveat, or question.
Lu et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: