Answers are grounded in this paper and cite their sources.
Geopolymer composites were synthesized with different Si:Al molar ratios and cured for different periods to investigate the correlation between phase transformation, microstructure evolution, and flexural strength. Phase transformation and microstructure evolution are correlated; sodalite content (72.8 wt%), i.e., kaolinite to sodalite transformation, is maximized at a Si:Al ratio (expressed as a decimal) of 1.94 and curing time of 24 h. The resulting products are characterized by a dense microstructure, and comparatively high relative density (54%) and flexural strength (20 MPa) owing to enhanced crosslinking and condensation during geopolymerization. However, increasing the Si:Al molar ratio to 2.22 reduces flexural strength to 16 MPa owing to a reduction in sodalite content (60 wt%) attributed to the impeditive effect of excessive silica on geopolymerization and the transformation of sodalite to cancrinite.
No takes yet. Share an insight, caveat, or question.
Gao et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: