Answers are grounded in this paper and cite their sources.
The setting of gypsum-based materials is governed by β-hemihydrate (β-HH) rehydration, yet a per-unit rate measurement is still lacking industrially. DFT places the four low-index faces of β-HH between 0.52 and 0.94 J m−2; the most stable, (010), is treated as the candidate rate-determining face. HPO42− binds to (010) 0.48 eV more strongly than water, whereas F− preferentially adsorbs on (001). Time-resolved XRD across four temperatures reveals two distinct kinetic stages; no single-exponent law is adequate, and the transition coincides with the end of the exothermic peak. Acoustic emission captures the same transition, with growth before and microcracking after, crossing at 34.1 ± 1.7 min. Acoustic energy tracks heat release almost linearly. A Bayesian observer built on this relation reproduced the Rietveld-derived degree of hydration on 48 specimens (R2 = 0.993; mean absolute percentage error 4.3%) and timed the stabilisation node at 96.8 ± 4.2 min against 95.4 ± 3.1 min by diffraction. On a board line (five days, 320 boards; before-and-after, not a controlled trial), the schedule driven by this measurement was associated with a lower strength coefficient of variation (4.6% vs. 8.4%) and lower curing energy (15.2 vs. 21.5 kWh m−2); restricting to inlet-temperature-matched days attenuated these to −38% and −22%.
No takes yet. Share an insight, caveat, or question.
Zhao et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: