In this work, the surface modification of AA6062 alloy was investigated by using electro-discharge coating (EDC) with powder metallurgy-based h-BN–Cu composite electrodes with h-BN weight ratios of 70:30, 50:50 and 40:60. The effects of electrode composition, peak current and pulse-on-time on surface morphology, roughness, elemental transfer, phase constitution, crystallographic characteristics and tribological performance were evaluated. SEM and 3D optical profilometry showed composition- and parameter-dependent surface characteristics, with the lowest areal roughness (Sa) of about 2.5 µm achieved with the 50:50 electrode. EDS analysis showed an increase in boron content from 18.30 to 49.39 wt.% with increasing h-BN fraction. XRD showed reflections for h-BN and Cu. The 50:50 composition resulted in a compact coating, a crystallite size of 9.5 nm and a dislocation density of 38 × 10¹⁴ m−². EBSD showed a composition-dependent Cu texture intensity (3.870–4.793 MRD), a nearly constant h-BN texture, and strong grain-boundary misorientation peaks at 40°–50°. The 50:50 electrode also showed the lowest wear rate of 0.000246 mm³/N·m at 15 A and the lowest coefficient of friction of 0.233. The surface microhardness increased significantly from 87 HV for the uncoated alloy to 308 HV after coating.
No takes yet. Share an insight, caveat, or question.
Sethi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: