PbTiO₃ is a typical ferroelectric polarization induced negative thermal expansion (NTE) material at a wide range of temperature. The elegant TiO₆ octahedron is used to study the polarization and NTE, whereas lacking its quantitative characterization. In this work, we propose a concise projection of vibrational amplitude to describe anisotropic distortion of atoms with temperature based on $ab$ $initio$ molecular dynamics simulations. We find that the huge negative mode Grüneisen coefficient is mainly from the different vibrational modes of the TiO₆ octahedral rotation at two boundary symmetry points in tetragonal phase along c direction. The potential energy surface as a function of amplitude suggests the c-axis compression facilitates the TiO₆ octahedral rotation. We show that the vibrational mode of TiO₆ octahedral rotation around negative-expansion axis can promote spontaneous polarization reduction with increasing temperature, making transformation of PbTiO₃ from tetragonal to cubic phase occur, via the projected amplitude, potential energy surface, and forces of individual atoms.
No takes yet. Share an insight, caveat, or question.
Gao et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: