Answers are grounded in this paper and cite their sources.
Functionally graded aluminium matrix composites reinforced with TiB 2 were produced through horizontal centrifugal casting. The TiB 2 phase was generated in situ by the reaction of K 2 TiF 6 and KBF 4 salts within the molten aluminium. Hollow cylindrical composites containing a fixed 7.5% of TiB 2 were cast at rotational speeds of 1000, 1100 and 1200 r/min. The effects of varying mould speeds on the mechanical, tribological and corrosion properties of Al–TiB 2 functionally graded composites were examined and compared to those of pure aluminium. The microhardness improved with the addition of TiB 2 reinforcement, with further increases observed at higher mould speeds. The composite fabricated at 1100 r/min exhibited superior tensile strength and wear performance, and it also showed the highest corrosion resistance compared to the other samples.
No takes yet. Share an insight, caveat, or question.
Rajak et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: