To investigate changes in interfacial quality and mechanical strength during seawater exposure, this study examines the degradation behavior of 3D‐printed glass‐fiber‐reinforced polyamide 6 (GF/PA6) composites under accelerated seawater aging. Four key process parameters (layer thickness, printing speed, printing temperature, and line width) were selected as inputs to a BP neural network prediction model optimized using particle swarm optimization (PSO). The non‐dominated sorting genetic algorithm (NSGA‐II) was employed for multi‐objective process optimization. Accelerated seawater aging tests were conducted on GF/PA6 composites prepared using the selected process schemes to evaluate changes in performance and structure at different aging stages. The results show that GF/PA6 composites prepared with different process parameters exhibit deteriorated interfacial quality and reduced mechanical strength after seawater aging. Notably, a 37.86% decrease in tensile strength indicates that seawater aging significantly affects the composites, and changes in surface morphology and microstructure were also observed after aging. When the printing parameters are set to a layer thickness of 0.1 mm, printing speed of 45 mm/s, printing temperature of 286°C, and line width of 0.42 mm, the GF/PA6 composites exhibit better mechanical properties and water resistance.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: