In this study, polyethylene glycol 400 and ethylene glycol were used as the copolymerization liquidation agents, and concentrated sulfuric acid was used as the catalyst. The corn straw (CS) was liquefied at 160 °C under normal pressure. 2-methylimidazole was used as the curing agent to prepare the liquefaction product (LP)/E51 composite material. The structure of the liquefaction product was characterized by Fourier transform infrared spectroscopy and gas chromatography-mass spectrometry coupling, and the scanning electron microscope, differential scanning calorimetry, thermogravimetry and mechanical properties tests were conducted for different epoxy systems. The experimental results showed that adding different proportions of LP to E51 could improve its toughness and strength to varying degrees. When the LP addition amount was 20 wt%, the impact strength of E51 reached the maximum value of 11.14 kJ/m2, which was 499.1% higher than that of pure E51. When the LP addition amount was 15%, the tensile strength (44.61 MPa) was 300.81% higher than that of pure E51 (11.13 MPa), and the bending strength increased from 17.43 MPa (pure E51) to 98.95 MPa. The experimental results indicated that LP was a mixture of different chain-length molecules with terminal hydroxyl groups, which significantly reduced the activation energy required for the curing of the system. The toughness and mechanical strength of E51 were significantly enhanced. It is notable that the glass transition temperature (Tg) determined by DMA decreased from 174 °C to 80 °C, indicating an increase in flexibility; while the initial thermal decomposition temperature (Td5%) determined by TGA slightly decreased.
No takes yet. Share an insight, caveat, or question.
Lou et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: