Answers are grounded in this paper and cite their sources.
Type-IIA diamond single crystals containing approximately 0.1%, 0.5%, and 1% ¹³C were synthesized and their thermal diffusivities were measured at room temperature by the thermal-wave-mirage technique. The measured value (18.5 cm²/s) of the 0.1% ¹³C crystal was 50% higher than the 1% ¹³C (natural isotope abundance). This is the highest room-temperature thermal diffusivity of any solid naturally occurring or previously synthesized. The laser damage threshold at 193 nm for the isotopically enriched crystal is more than an order of magnitude higher than that of natural diamond.
No takes yet. Share an insight, caveat, or question.
Anthony et al. (1990) studied this question.