Highly porous anodic alumina (PAA) was prepared by anodic oxidation of an aluminum substrate at room temperature. The research investigated how the pore size and porosity of PAA were affected by substrate and anodization factors during the preparation process. Substrate factors included substrate purity and substrate heat treatment; anodization factors mainly focused on parameters of the anodizing process (anodization voltage, electrolyte solution type, electrolyte solution concentration, bath temperature, and anodic oxidation time). The PAA membrane was used for cell culture (MG63 cells) and cell viability was assessed using the microculture tetrazolium method. The effects of different pore sizes of PAA membranes on cell morphology were observed using scanning electron microscopy (SEM) at observation times of 4 hours, 1 day, 4 days, and 7 days. The results showed that regardless of the electrolyte solution, the pore size (25-150 nm) and porosity (50-75%) of PAA increased with increasing anodic oxidation voltage (20-60 V), bath temperature (5-25 °C), and electrolyte concentration (0.1-1.0 M). However, the anodization voltage cannot be increased indefinitely; otherwise, PAA fabrication will fail and the porous structure will not be achieved. Cell culture showed that the cell attachment had enhanced as the pore size (120 nm) of the PAA increased.
No takes yet. Share an insight, caveat, or question.
Huang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: