Hybrid polyether ether ketone–carbon fibre–TiB 2 (PEEK–CF–TiB 2 ) composites were investigated to elucidate the coupled influence of TiB 2 loading (0–3 wt%) and melt‐mixing duration (30 and 40 min) on crystallization, microstructural evolution and dielectric response. In the K30 series, TiB 2 promoted heterogeneous nucleation, increasing the crystallization temperature from 273.3 to 281.2 °C at K30‐2, while the crystalline fraction increased from 40.4% to a maximum of 49.9% at K30‐3. Prolonged mixing produced a distinct thermal response in the K40 series, characterized by a progressive increase in glass transition temperature from 155 to 174 °C and a non‐monotonic evolution of crystallinity. Field‐emission scanning electron microscopy revealed a finer and more spatially distributed particulate morphology after prolonged mixing, while X‐ray diffraction confirmed retention of the characteristic crystalline phases and processing‐dependent variation in PEEK crystalline ordering. Isothermal thermogravimetric analysis established high mass retention throughout the processing‐relevant thermal exposure. Dielectric spectroscopy showed an increase in dielectric constant from 487 to 836 at 1 kHz across the K40 series, accompanied by controlled loss‐tangent values and frequency‐dependent conductivity characteristic of an interfacial‐polarization‐dominated electrical regime. The combined thermal, morphological, crystallographic and dielectric results demonstrate that melt‐mixing duration regulates the balance between heterogeneous nucleation, segmental constraint and Maxwell–Wagner–Sillars polarization in hybrid PEEK–CF–TiB 2 composites.
No takes yet. Share an insight, caveat, or question.
Dahiwal et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: