The functional role of Pd in ZnO-based materials depends on the wurtzite host response, the formation of Pd-containing secondary phases, and the evolution of surface and interfacial environments. Here, we investigated ZnO-based materials with nominal Pd contents of 0, 1, and 5% to determine how this compositional evolution affects lattice response, surface electronic states, optical behavior, and metronidazole (MET) photocatalytic removal. Rietveld refinement showed a modest expansion of the ZnO lattice at 1% Pd, increasing the unit-cell volume from 47.30 to 47.53 Å 3 , whereas increasing the nominal Pd content to 5% primarily increased the PdO and Pd phase fractions without further expansion of the wurtzite cell. X-ray photoelectron spectroscopy revealed progressive changes in the near-surface Zn–O electronic environment, with the Zn 2p and lattice-oxygen core levels shifting to higher binding energies as the Pd content increased. Pd 3d components corresponding to metallic Pd 0 and Pd 2 ⁺ associated with PdO, together with an intermediate-binding-energy contribution consistent with electron-deficient Pdδ⁺ environments, were resolved. The relative fitted area of this intermediate Pd component increased from 58.3 to 73.7% between 1 and 5% Pd, while the relative area of the high-binding-energy O 1s component increased from 7.1 to 27.9%. Urbach energy increased from 62.7 to 79.7 meV with increasing Pd content, consistent with a broader distribution of localized electronic environments. Among the investigated compositions, the nominal 1% Pd sample showed the highest photocatalytic activity, reaching 86% apparent MET removal after 120 min, compared with 56% for pristine ZnO and 80% for 5% Pd. The corresponding k app was 1.65 × 10 −2 min⁻ 1 , approximately 2.3 and 1.2 times the values obtained for pristine ZnO and 5% Pd, respectively. The largest activity loss occurred under hole scavenging, with MET removal decreasing from 86 to 57%, while MeOH and CHCl 3 reduced the conversion to 63 and 70%, respectively. These results support the participation of hole-dependent oxidation, •OH-mediated chemistry, and electron-dependent O 2 reduction, with the strongest inhibition observed under hole scavenging. Reusability tests showed an initial decrease in MET removal from 86 to 42% after the first recovery, followed by a nearly stable response of 41% in the third cycle; post-use Raman spectroscopy and elemental mapping confirmed the persistence of ZnO and PdO signatures and dispersed Pd. Acute-toxicity assays using Artemia salina showed 100% survival after both 24 and 48 h for the aqueous phase treated with 1% Pd. Within the investigated series, the nominal 1% Pd composition provided the most favorable balance between lattice response, surface and interfacial environments, photocatalytic kinetics, and high Artemia salina survival after treatment.
No takes yet. Share an insight, caveat, or question.
Silva-Benigno et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: