In this study, we systematically evaluated the densification behavior, microstructural evolution, and magnetic properties of Nd-Fe-B compacts processed by Electrically Heated Powder Rolling (EPR) in 1 to 5 rolling passes at a constant current of 1000 A and a rolling speed of 0.3 mm/s. The EPR conditions enabled rapid consolidation: the reduction rate increased from 67.0% after 1 pass to 74.0% after 3 passes and 76.3% after 5 passes, corresponding to an increase in relative density from 71% to 91% and 95%, respectively. The highest coercivity of 221 kA/m was obtained at 74% reduction (3 passes), where the Nd-rich phase was relatively well distributed along intergranular regions, while the microstructure still suggested insufficient formation of a continuous nanoscale Nd-rich grain-boundary phase. Because temperature control during EPR is not yet fully optimized, the present processing conditions do not maximize the intrinsic potential of Nd-Fe-B magnets. Overall, the results demonstrate that effective densification and partial sintering of Nd-Fe-B can be accomplished within minutes by Joule heating-driven rolling, highlighting the high efficiency and promise of the EPR process.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: