As semiconductor devices scale to the nanometer level, high-k metal gate (HKMG) technology is widely adopted, but power consumption becomes problematic due to effective work function (EWF) shifts caused by interface dipoles at high-k dielectrics. Inserting an Al2O3 layer at the dielectric/gate interface reduces power consumption by adjusting the EWF, but it significantly slows W gate deposition. Experimentally, introducing a TiN layer on Al2O3 promotes fast and uniform W growth, yet the underlying mechanism remains unclear. Here, density functional theory calculations reveal the nucleation and growth of W on Al2O3 and TiN surfaces. We identify stable AlO(II)-terminated Al2O3(001), TiN(001), and N-terminated TiN(111) surfaces and their most stable W adsorption sites. As more W atoms adsorb, a W cluster forms on Al2O3 and a W nanosheet develops on TiN, with stronger W adsorption on TiN during nucleation. In the growth step, W binds more strongly to the W nanosheet than to the W cluster, further accelerating W deposition. These strong W adsorption on TiN are attributed to the robust W-N bonding, forming uniform W metal nanosheets. Our findings clarify the nucleation and growth mechanisms of W deposition and suggest the optimal surface for cost-efficient HKMG production with improved electrical performance.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: