Answers are grounded in this paper and cite their sources.
Resin-based composites (RBCs) may change mechanically during prolonged aqueous storage, while residual monomers and related low-molecular-weight compounds can be released from their polymer networks. This study evaluated four conventional and four bulk-fill RBCs. Engineering compressive modulus, maximum engineering compressive stress, and engineering strain at maximum engineering compressive stress were determined after 24 h and after 20 weeks of storage in physiological saline. Extraction of selected compounds was quantified by HPLC after 1, 2, 4, 8, and 20 weeks in 75% ethanol/water. Compressive properties changed in a strongly material-dependent manner between the 24-h and 20-week saline-storage conditions, ranging from reductions to stable behavior or increases in selected parameters, particularly among bulk-fill RBCs. Material composition, extraction time, and their interaction significantly affected cumulative monomer extraction. These findings show marked material-dependent variation in both outcomes and indicate that conventional and bulk-fill classification alone does not predict compressive-property changes after prolonged saline storage.
No takes yet. Share an insight, caveat, or question.
Lempel et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: