Solid‐state zinc batteries are promising for safe and low‐cost energy storage, yet the subzero operation is hindered by sluggish Zn 2+ transport, unstable electrode/electrolyte interfaces, and nonuniform Zn deposition. Herein, a zwitterionic ion‐pair decoupling strategy is introduced into the PVDF‐HFP/Zn(OTf) 2 /EC polymer electrolyte by incorporating 2‐methacryloyloxyethyl phosphorylcholine (MPC), thereby coupling bulk solvation regulation with interfacial crystallographic modulation. The bulky methacrylate side chain disrupts ordered PVDF‐HFP packing and promotes amorphous ion‐conducting domains. Meanwhile, the spatially separated quaternary ammonium and phosphate oxygen moieties redistribute OTf − and moderately coordinate Zn 2+ , respectively, weakening Zn 2+ ‐OTf − ion pairs and accelerating Zn 2+ solvation exchange and migration. Moreover, this strategy directs preferential Zn(002) texture evolution, enabling compact and dendrite‐free deposition. Consequently, the MPC‐modified electrolyte sustains stable Zn plating/stripping for 2000 h at 0.1 mA cm −2 . Remarkably, Zn|VO 2 cells retain a capacity of 78 mAh g −1 after 2800 cycles at 0.2 A g −1 under −20°C. This work establishes a molecular design principle that links ion‐pair chemistry, interfacial kinetics, and crystallographic deposition in subzero solid‐state zinc batteries.
No takes yet. Share an insight, caveat, or question.
Wen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: