Answers are grounded in this paper and cite their sources.
This study investigates the mechanical performance and accelerated hydrothermal seawater durability (60 °C) of cement mortar incorporating crushed oyster shells (OS, <2.0 mm) as a fine aggregate replacement for natural quartz sand at 0%, 25%, 50%, and 100% levels. Standard prisms (40 × 40 × 160 mm) were tested under standard potable water curing, continuous 60 °C seawater curing (7 and 28 days, benchmarked against 20 °C potable control), and accelerated 60 °C hydrothermal seawater immersion (2, 4, and 8 wk) per BS EN 196-1:2016. Under standard curing, compressive strength increased monotonically with OS content to 34.81 MPa (+59.1% over control) at 100% replacement. Continuous 60 °C seawater curing accelerated early-age hydration (+24.4% at 7 days vs. control). Under accelerated 60 °C seawater exposure, 100% OS mortar attained 39.38 MPa in compression (+79.0% over unexposed control) and 7.97 MPa in flexure at 8 wk. A robust power-law correlation linked flexural and compressive strength (ffl = 0.91·fc^0.58, R2 = 0.83). Time-resolved FTIR spectroscopy confirmed the persistence of polymerised C–S–H gel and enhanced carboaluminate formation without expansive ettringite distress. Crushed oyster shells represent a viable, sustainable replacement for natural fine aggregates in coastal construction.
No takes yet. Share an insight, caveat, or question.
Shamseldein et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: