Answers are grounded in this paper and cite their sources.
Thermal pyrolysis of polyethylene (PE) under pressure and hydroisomerization over Pt/SAPO-11 are known separately; this work examines their integration. PE was pyrolyzed at 400–550 °C and constant pressures of 0.1–2.0 MPa, and the 140–280 °C fraction (pyrolysis kerosene) was hydroisomerized over 0.5 wt% Pt/SAPO-11. The yield of the 140–280 °C fraction decreases with temperature and increases with pressure, reaching 45.3 wt% at 400 °C and 1.0 MPa (27.4 wt% at 0.1 MPa); a control run under these conditions gave a directly measured gas yield of 13.2 wt% and a mass balance closure of 99.3%. The pyrolysis kerosene contains 47.6 wt% alkenes and 20.0 wt% cycloalkanes. Hydroisomerization at 6 MPa and a liquid hourly space velocity of 3 h−1 gives 91.1–93.4 wt% of the kerosene fraction (>140 °C) at 290–300 °C, with near-complete alkene hydrogenation; at 330 °C, the freezing point falls below −90 °C (pyrolysis kerosene: −13 °C), but hydrocracking reduces the yield to 72.4 wt%. The kerosene fraction obtained at the selected temperature of 300 °C (57.2% isoalkanes, 25.1% cycloalkanes, 0.1% aromatics) meets all measured GOST 10227-86 requirements for Russian RT jet fuel except density. The overall kerosene yield is 41.3 wt% of PE (40.0–40.4 wt% within the 140–280 °C boundaries). A preliminary estimate shows that the heat and hydrogen demand of the process corresponds to 68–97% of the energy of the pyrolysis gases.
No takes yet. Share an insight, caveat, or question.
Yakovenko et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: