This study compares the tensile properties and microstructural constituents of EN-1561-GJL-300 (lamellar graphite iron) and EN-16079-GJV-300 (compacted/vermicular graphite iron) on the basis of experimental tensile testing. metallographic analysis. control-volume casting-process simulation. and finite-element tensile-test simulation. Cast Y-block specimens were produced in furan-bound sand moulds at 1400–1410°C from two separate melts. Tensile tests were carried out in accordance with EN 1561 and EN 16079 on a minimum of ten specimens per material at a crosshead speed of 1 mm·min⁻¹. Following the exclusion of one specimen per material due to casting discontinuity, nine valid tensile-test results (n = 9) were included in the statistical evaluation for each material. Brinell hardness was measured at ten locations on each specimen (3000 kgf. 10 mm steel ball). and microstructure was quantified on at least 15 fields of view per condition. both as-polished (graphite morphology) and after 2% nital etching (matrix phases). The experimental melt for GJL-300 exhibited a tensile strength of 256 MPa. predominantly Type-A flake-graphite morphology (≥ 90% of evaluated fields). 15 vol.% graphite. an elongated graphite length fraction of 45%. and a matrix of approximately 71% pearlite / 29% ferrite. The experimental melt for GJV-300 exhibited a tensile strength of 313 MPa. 8% nodularity (ASTM A247). 12 vol.% graphite. and a matrix of approximately 89% pearlite / 11% ferrite. For EN-16079-GJV-300, the deviations between the experimental results and the CV and FE simulations were 35.8% and 7.2%, respectively. For EN-1561-GJL-300, the corresponding deviations were 30.9% and 8.9%, respectively. The markedly smaller deviation of the FE results is attributable to the use of the actual tensile-specimen geometry and identical boundary conditions rather than the as-cast Y-block cross-section employed in the CV workflow. Cooling-curve analysis indicates full solidification at approximately 250 s for GJL-300 (with a graphitisation interval of about 180 s) and approximately 184 s for GJV-300 (graphitisation interval of about 88 s). consistent with the measured higher graphite volume fraction and longer flake length of the GJL-300 melt. The proposed combined workflow provides a validated methodology for selecting engine-block materials by integrating casting-process simulation, finite-element analysis, and experimental characterization.
No takes yet. Share an insight, caveat, or question.
Uluç et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: