Answers are grounded in this paper and cite their sources.
High-density mortar coatings are increasingly used to shield medical and industrial radiation facilities. Ten cement mortars were prepared at water-to-cement ratio 0.60, with fine aggregate partially replaced by barite powder, steel powder, or both at 10, 20 and 30 wt.%. Density, 28-day compressive strength and the linear attenuation coefficient were determined, the latter in narrow-beam geometry with a NaI(Tl) detector using 133Ba, 137Cs and 60Co at 0.356, 0.662, 1.173 and 1.332 MeV, and compared with WinXCom. All modified mortars were denser (2.06–2.29 versus 2.01 g/cm3) and stronger than the control. Best shielding came from 30% barite powder and from 20% barite powder with 10% steel powder, giving μ of 0.244 and 0.241 cm−1 at 0.356 MeV, statistically indistinguishable. The latter also gave the highest strength, 58% above the control, and reduced the half-value layer by 14.9% at 0.356 MeV. μ correlated strongly with density (R2 = 0.937–0.998), most weakly at 0.356 MeV where the high atomic number of barium enhances photoelectric absorption. WinXCom overestimated μ by 3.08 to 10.75%, the deviation reflecting entrapped air, not cross-section error. Combining both powders therefore matches the shielding of higher single-additive dosages at lower heavy-aggregate content while improving strength.
No takes yet. Share an insight, caveat, or question.
Prapan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: