Answers are grounded in this paper and cite their sources.
Al-, Ga-, and In-doped tin monoxide (SnO) films were grown by molecular beam epitaxy. Hall measurements reveal acceptor character of all investigated group-III dopants in SnO, which corresponds to theoretical calculations and previous experiments for Ga and In, but contradicts theoretical calculations predicting donor character for Al in SnO. Doping concentrations of 1018–1022 cm−3 were tested and maximum hole concentrations of 2×1019, 3×1019, and 1×1019 cm−3 with doping efficiencies of 3%, 9%, and 1% were found for Al, Ga, and In, respectively. The observed doping limit in the mid 1019 cm−3 aligns with the limits observed in literature for different dopants, hinting to fundamental aspects of the SnO defect chemistry. Due to the unexpected Al acceptor behavior, we hypothesized Al1+ being present instead of Al3+. To stabilize the higher Al3+ oxidation state, another sample series of Al-doped SnO was grown in an oxidizing atmosphere. Despite the oxidizing atmosphere, these samples showed p-type character. A more complex defect chemistry is thus expected to explain the Al acceptor character.
No takes yet. Share an insight, caveat, or question.
Gutmann et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: