The development of polymer dielectrics with high energy density, low loss, and high‐temperature reliability remains challenging for advanced film capacitors. Conventional polyimide (PI) dielectrics suffer from high dielectric loss and limited breakdown strength, restricting their energy storage capability at elevated temperatures. This study proposes a “rigidity–flexibility integration” strategy by chemically incorporating flexible Poly(dimethylsiloxane) bis(3‐aminopropyl) terminated (PDMS) segments into rigid PI backbones. Systematic investigation demonstrates that PDMS effectively modulates dielectric response and breakdown characteristics. The optimized PI‐PDMS copolymer composite films exhibit a 44% reduction in dielectric loss (from 0.008 to 0.0045) and a 27% enhancement in breakdown strength (from 365 to 467.9 MV/m), while maintaining a dielectric constant of ~3.3. Consequently, the copolymer composite films achieve a discharged energy density of 4.0 J/cm 3 at room temperature and retain 2.6 J/cm 3 with over 80% efficiency at 150°C, alongside excellent cycling stability over 100,000 cycles. These improvements originate from deep‐level traps and tailored free volume introduced by PDMS segments, which suppress charge transport and polarization loss. This work provides an effective strategy for designing high‐performance polymer dielectrics with balanced properties and outstanding high‐temperature reliability for capacitive energy storage.
No takes yet. Share an insight, caveat, or question.
Zhen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: