Answers are grounded in this paper and cite their sources.
The patterns of water leaching of chlorides depending on temperature, liquid-to-solid ratio (hydromodule), and time were studied using samples of dust emissions from gas cleaning in electric steelmaking production at the Abinsk Electric Steel Works, generated in 2022–2025. A water-leaching regime was established under which up to 98.6% of chlorides are extracted. A method for purification of the washing waters after leaching was proposed, reducing the calcium content by 99.6% and lead content by 92%, and the pH of the filtrate to 8–9 without the use of additional reagents; at the same time, the purified water becomes suitable for further use in the technological cycle. It was noted that the dry residue of the filtrate, consisting of 75–85% potassium and sodium chlorides, is suitable for technical use, while the solid residue of gas-cleaning dust waste after water leaching is a concentrate containing 34.0% Zn and 24.5% Fe, which can be directed to Waelz processing or hydrometallurgical treatment.
No takes yet. Share an insight, caveat, or question.
Темердашев et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: