Vat photopolymerization (VPP) of SiC ceramics produces green bodies that contain about 45 vol% organic phase, so thermal debinding does not simply remove a fugitive binder but defines the pore architecture on which both the subsequent solid-state sintering and the pore-related functionality depend. This work examines how the debinding temperature (450–650°C) governs the open pore structure, the structural ordering of the residual carbon and the porosity–strength relationship of pressureless-sintered SiC ceramics. Mercury intrusion porosimetry shows that the open porosity rises from 27.25% at 450°C to a maximum of 35.92% at 600°C, with a single pore-size peak between 100 and 300 nm, while the total pore area falls from 9.07 to 2.67 m² g⁻¹, indicating that a tortuous, high-surface-area pore network is replaced by a coarser and better-connected one. EDS and Raman spectroscopy show that the residual carbon is progressively enriched and reaches its highest structural order at 600°C (ID/IG = 0.63). The ceramic debound at 600°C combines a sintered porosity of 13.99%, a density of 2.77 g cm⁻³ and a flexural strength of 290.2 ± 24.3 MPa, and the strength–porosity data follow the Ryshkewitch–Duckworth relation (σ0 = 394.9 MPa, b = 2.36, R² = 0.949). The debinding temperature therefore provides a single processing lever for the design of porous VPP-SiC components with a controlled open pore fraction and load-bearing capacity.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: