Continuous fiber-reinforced polymer composites offer significant potential for additive manufacturing, but achieving optimal fiber-matrix impregnation remains a critical challenge. This study addresses it by systematically investigating the effect of nozzle temperature and extrusion speed on the impregnation quality and tensile performance of continuous glass-fiber/PLA filaments fabricated via a custom co-extrusion setup. A full-factorial design with three temperatures (463, 483, 503 K) and three speeds (100, 150, 200 mm/min) was employed. SEM cross-sections were quantitatively analyzed to determine fiber volume fraction, resin fraction, void fraction, and an impregnation index, while tensile testing evaluated mechanical performance. Results demonstrated a strong process dependence: higher temperature and lower speed improved matrix impregnation, reducing void content and increasing tensile strength from 92.34 MPa to 146.72 MPa. ANOVA confirmed both factors were highly significant (p < 0.001) and the model explained 90.38% of the variance in tensile strength. Correlation analysis revealed strong relationships between tensile strength and impregnation index (r = 0.981) and between strength and void fraction (r = - 0.982). This study establishes the comprehensive process–structure–property relationship for continuous glass-fiber/PLA filaments, providing a quantitative framework for optimizing continuous-fiber additive manufacturing systems and enabling the production of high-performance structural components with predictable properties.
No takes yet. Share an insight, caveat, or question.
Nejkar et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: