Answers are grounded in this paper and cite their sources.
This study maps operational separation responses in cut fragments from one field-aged crystalline-silicon photovoltaic module containing a polyolefin elastomer (POE)-rich encapsulant. Through-glass irradiation used a 532 nm picosecond laser and eighteen combinations of repetition rate (100–300 kHz), controller setting (50% or 100%), and scan speed (1000–2000 mm s−1). After cooling, one operator assessed corner-initiated manual opening. Responses were classified by sustained opening, interface-opening sequence, and visually estimated released area. Two additional fragments were tested for each of four selected conditions. At 300 kHz and 1000 mm s−1, all three fragments at the 50% setting (G13) showed limited opening with perceived greater resistance, whereas all three at 100% (G16) showed direct release of the glass–POE package from silicon. All three G4 fragments reached full-area separation, with variable or indeterminate interface-opening sequence. A separate specimen processed at 600 kHz fragmented. Local SEM and EDS documented selected exposed silicon-side fields after opening. The resulting map identifies laser programs for gaining access to material interfaces for subsequent recovery studies. Recovery yield and functional product quality were not evaluated.
No takes yet. Share an insight, caveat, or question.
Tofil et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: