To improve the durability of cement-based materials in multi-salt coupled corrosion environments, six cement mortar mixtures were designed. The fly ash content ranged from 10% to 40%, and the superabsorbent polymer (SAP) content ranged from 0% to 0.3%. Four corrosion environments were used: tap water, 10% NaCl solution, 10% MgSO4 solution, and a 10% NaCl with 10% MgSO4 composite solution. The degradation behavior and the modification mechanism of fly ash and SAP were investigated. Macroscopic tests were performed on apparent morphology, mass change, compressive strength, and flexural strength. Thermogravimetric and derivative thermogravimetric (TG/DTG) analysis and scanning electron microscopy (SEM) were also conducted. It was found that the damage caused by multi-salt coupling was much greater than that caused by single-salt corrosion. The damage severity decreased in the order of composite solution, MgSO4 solution, NaCl solution, and tap water. The competitive adsorption, synergistic reactions, and mutual antagonism of Cl−, SO42−, and Mg2+ associated with large-area surface spalling, penetrating cracks, and mechanical strength loss. A parabolic trend was observed for the effect of fly ash content on corrosion resistance. The best balance between the filling effect and secondary hydration was obtained at a 20% content. The lowest mass loss and the highest compressive strength retention were obtained at this content. A 10% content was insufficient for modification. Corrosion resistance decreased at a 40% content because of the low clinker proportion. An optimal SAP content threshold of 0.2% was observed. With an appropriate SAP content, the pore size was refined, connected pores were blocked, and the expansion stress of corrosion products was buffered. Corrosion damage was thereby delayed. The microscopic analysis indicated that more expansive products were formed under the multi-salt environment. These products included ettringite, gypsum, and Friedel’s salt. The C-S-H gel was also more severely damaged. With the combined addition of fly ash and SAP, the formation of corrosion products was reduced, the gel skeleton was protected, and a denser and more uniform microstructure was obtained. Therefore, a multiple protection system was formed by the combined addition of fly ash and SAP. This system involved physical blocking, chemical consumption, ion immobilization, and crack inhibition. The mixture with 20% fly ash and 0.2% SAP was the optimal mix proportion within the tested mixture series and exposure conditions. The durability of cement-based materials in the multi-salt coupled corrosion environment was improved within the tested mixture series and exposure conditions. An experimental basis for mix design and durability protection of cement-based materials in corrosive environments is provided by these findings.
No takes yet. Share an insight, caveat, or question.
Zheng et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: