Answers are grounded in this paper and cite their sources.
Background Branch wood is often discarded or used as fuelwood because its properties are insufficiently documented. This study compared stem and branch wood of Samanea saman , distinguishing heartwood from sapwood, to assess the potential of branch wood for structural and furniture applications. Methods Ten stem logs and ten branch logs were sampled from natural forest in Ghana. Moisture content and oven-dry density were determined using European Standard EN 13183-1 (2002) and the International Organization for Standardization method ISO 3131 (1975), respectively. Static bending, compression parallel to the grain and shear parallel to the grain were tested in accordance with British Standard BS 373:1957. Data were analysed using repeated-measures analysis of variance and least significant difference pairwise comparisons. Results Wood portion significantly affected all measured physical and mechanical properties. Moisture content ranged from 69.50% in stem heartwood to 85.50% in branch sapwood. Branch heartwood had the highest oven-dry density (819.10 kg/m 3 ), while stem heartwood had the highest modulus of elasticity (12,214.19 MPa) and modulus of rupture (118.55 MPa). Branch heartwood recorded the highest compressive strength (60.60 MPa) and shear strength (18.93 MPa). Branch heartwood did not differ significantly from stem heartwood in modulus of rupture or compressive strength. Conclusions Stem heartwood showed the highest stiffness and bending strength. Branch heartwood demonstrated comparable performance to stem wood for selected strength properties and may be suitable for furniture components, joinery and moderately loaded applications. Branch sapwood is more appropriately considered for non-structural uses.
No takes yet. Share an insight, caveat, or question.
Narh et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: