Aiming at the performance regulation demand for high-grade thin-gauge non-oriented electrical steel, 0.25 mm thick non-oriented electrical steel containing 3.53 wt.% Si was taken as the research object to investigate the effects of annealing temperature ranging from 850 °C to 1000 °C on its microstructure, texture characteristics, precipitates and magnetic properties. The results show that with increasing annealing temperature, the recrystallized grain size of the specimen increases first and then decreases, and the average grain size reaches a peak of 161.376 μm at 975 °C. At 950 °C, favorable textures including 4.6% {110}<001> Goss texture and 3.58% {001}<350> texture are formed, yielding the maximum magnetic flux density B50 of 1.865 T and a core loss P1.0/400 of 10.85 W/kg. The specimen annealed at 950 °C has a coercivity Hc of 62.64 A/m and a remanence Br of 515.2 mT. Overall, annealing at 950 °C achieves the optimal matching of magnetic induction and core loss for this thin-gauge non-oriented electrical steel. The research results can provide theoretical and data support for optimizing the annealing process of high-grade non-oriented electrical steel.
No takes yet. Share an insight, caveat, or question.
Lu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: