The oxygen reduction reaction (ORR) in protonic ceramic fuel cells (PCFCs) proceeds within H + /O 2− /e − triple‐conducting oxides. While facile bulk proton diffusion is conventionally assumed to spread the active reaction zone ( L eff ) throughout the porous electrode, the precise link between molecular‐level rate‐determining steps and this macroscopic spatial extent remains elusive. Here, we reveal this interplay by bridging atomic‐scale kinetics with macroscopic spatial utilization. By coupling in situ modulation‐excitation infrared spectroscopy with hydrogen/deuterium isotope‐resolved impedance analysis, we identify the vacancy‐assisted dissociation of accumulated superoxide () into active O − species as the molecular‐scale rate‐determining step. Integrating these surface kinetics with porous‐electrode theory reveals that this O − formation acts as an interfacial kinetic sink, consuming protons near the electrolyte interface before they penetrate the electrode bulk. Consequently, the overall ORR is confined to only a ∼110 nm zone in state‐of‐the‐art PrBa 0.5 Sr 0.5 Co 1.5 Fe 0.5 O 5+δ (PBSCF) cathodes at 600°C, leaving ∼98% of the porous scaffold electrochemically inert. This interfacial proton barrier is directly observed by time‐of‐flight secondary ion mass spectrometry isotope tracking on dense model films. Overcoming the interfacial proton exchange barrier to expand L eff , rather than solely accelerating surface kinetics, defines a design principle for state‐of‐the‐art PBSCF and potentially other porous mixed‐conducting electrodes.
No takes yet. Share an insight, caveat, or question.
Naik et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: