Polyurethane elastomers (PUEs) with systematically varied hard‐segment content and cross‐linking density were developed to investigate the relationship between mechanical balance and damage mechanisms under harsh service conditions. Structural and mechanical analyses reveal that molecular design controls stress distribution, inter‐segment mobility, and energy dissipation pathways, which together determine resistance to surface degradation. Moderate cross‐linking enables efficient load transfer while maintaining sufficient chain mobility, thereby suppressing the damaging from cavitation. During abrasion, two dominant damage modes operate concurrently: cutting‐induced material removal caused by hard abrasive particles, and strain‐induced failure resulting from localized deformation when the strain exceeds the material's elongation at break. The latter is strongly influenced by the ductility of the soft segments, while the former correlates with surface hardness. This work provides mechanistic insight into how tailoring molecular architecture enables a unified failure‐mitigation strategy, offering guidance for the design of durable polymer coatings in demanding fluid environments.
No takes yet. Share an insight, caveat, or question.
Li et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: