Duplex stainless steels (DSSs), containing roughly equal amounts of ferrite and austenite, offer an attractive combination of high strength and good corrosion resistance. The kinetics and factors controlling how fully ferritic material at temperatures near the solidus regains the desired 50/50 duplex microstructure around 1100 °C have previously been explored. The most important factor is nitrogen, present in the alloy, weld filler, and shielding gas. Other important factors are ferrite grain size and cooling rate, both influencing the time available for austenite formation at temperatures > 1000 °C, where kinetics remain favorable. Undesired intermetallic phases may form if the cooling rate is too slow, whereas rapid cooling rates and large ferrite grains promote chromium nitride precipitation. This study uses computational thermodynamics and the diffusion module DICTRA within Thermo-Calc to investigate how austenite formation influences nitride precipitation. The work focuses on the lean duplex grade LDX 2101, super duplex 2507, and 2509 weld metal filler. The simulations explore the influence of nitrogen content, grain size, and cooling rate on nitride precipitation. Furthermore, the commonly applied linear cooling rate in simulations is compared with non-linear conditions to evaluate their influence on nitride precipitation. Finally, the methodology developed in this work was applied to experimental data from a published study. Good agreement was obtained using the critical austenite spacing required for nitride precipitation as the comparison criterion. The simulations also reproduced the formation of nitride-free zones adjacent to austenite, indicating that high peak temperatures are required for these to form.
No takes yet. Share an insight, caveat, or question.
Wessman et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: