Joining operations in wax pattern manufacturing for investment casting are still performed manually, although they require high reproducibility, precise positioning and controlled material application. This study addresses whether collaborative robotics can be used for dip-and-push wax joining and evaluates the resulting process capability and reproducibility. Joints were evaluated by visual inspection, geometric measurement, adhesive wax loss and tensile testing. Two specimen geometries (14 mm and 21 mm), three wax bath temperatures (80–100 °C) and three dwell times (1–30 s) were investigated in 180 joining operations. The robot-assisted joining process proved to be reproducible and process-stable, with bonding defects in 2 of 180 joints (1.1%). Mean misalignment (0.28–0.76 mm) meets the tolerance for attaching feeders and gates by a wide margin (Ppk > 10) but not yet that for high-precision joints. Mean tensile forces were 105–182 N (14 mm) and 250–467 N (21 mm). Bead bubbles occurred only in 14 mm joints (57%), protrusions only in 21 mm joints (46%) and all joints exhibited adhesion failure. Specimen geometry was the dominant influencing factor, whereas no clear linear influence of wax bath temperature or dwell time was identified.
No takes yet. Share an insight, caveat, or question.
Wiese et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: