This research investigated the response of geopolymer reinforced concrete beams considering different span lengths, cross-sectional dimensions, and longitudinal reinforcement. A total of seven beams, designated D1–D7, were tested, with beam lengths ranging from 450 to 600 mm and depths from 150 to 450 mm. The compressive strength of the geopolymer concrete was 25.9 MPa, achieved under ambient curing conditions. All beams were also ambient cured and subsequently tested under three-point bending, exhibiting peak loads between 53.80 and 236.70 kN. With shear-span-to-beam-depth ratios (a/h) varying from 0.33 to 1.50, the tested beams exhibited predominantly shear-controlled behavior, characterized by diagonal cracking and shear-dominated failure. The experimental results were also compared with analytical predictions to evaluate the applicability of existing design approaches to the tested geopolymer concrete beams. The use of geopolymer concrete without heat curing eliminates the need for an additional heat-curing process and may facilitate practical on-site casting.
No takes yet. Share an insight, caveat, or question.
Phan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: