During the operation of the tokamak device, the high heat load released by the core plasma instability events severely affects the structure and performance of tungstenbased divertor materials. For the expected Type I ELMs in future long-pulse steadystate fusion devices, the coaxial gun discharge plasma parameters are designed to simulate the characteristics of low-medium energy density. Under constant initial conditions (discharge frequency, gas-prefilled), the total accumulated heat flux is kept constant by varying the energy density and the number of pulses. By combining the plasma-material interaction process, the temperature evolution of tungsten (W) target under different heat loads and its damage effects are comparatively studied. The results show that when the total energy is fixed, the thermal deposition time scale and the instantaneous temperature gradient lead to different types of damage, including roughening, grain loss, blistering, crack networks, and cracking accompanied by melting. Low-energy-density multi-pulse impacts cause slow heat deposition and small temperature gradients, increasing surface roughness via cyclic thermal stress. Highenergy-density impacts involving only a few pulses cause rapid heat deposition and steep temperature gradients, inducing high thermal stresses that lead to blistering and cracking. The energy density of an individual pulse determines the transition from surface to bulk damage. These results suggest that peak heat load control should take priority over cumulative heat flux limitation in the service design of W targets for fusion devices.
No takes yet. Share an insight, caveat, or question.
Qi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: