Answers are grounded in this paper and cite their sources.
Developing Fe‐rich 2:17‐type SmCo magnets (Fe ≥ 20 wt.%) with high energy products remains a significant challenge, because increasing Fe content progressively aggravates the competitive nucleation disadvantage of the SmCo 5 (1:5H) phase and promotes nanoscale discontinuity of the Cu‐rich 1:5H cell walls. Herein, a synergistic nucleation–composition (SNC) modulation strategy is proposed to precisely govern the early‐stage competitive nucleation kinetics in Fe‐rich SmCo magnets. By preserving defect‐assisted nucleation sites, rapidly accessing the effective 1:5H nucleation temperature regime, and promoting concurrent Cu partitioning, the SNC strategy favors early 1:5H nucleation and subsequent formation of continuous Cu‐rich cell walls. Consequently, the Sm 25 Co 45 Fe 23 Cu 4 Zr 2 (wt.%) magnet delivers a remarkable maximum magnetic energy product of 35.06 MGOe, together with a remanence of 12.24 kGs and an intrinsic coercivity of 19.76 kOe. This work establishes the critical importance of early‐stage phase decomposition in regulating cell‐wall formation, providing a synergistic pathway through synchronized nucleation kinetics and compositional partitioning for Fe‐rich 2:17‐type SmCo magnets.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: