An ultrahigh-Zn Al–15Zn–3Mg–1.5Cu–0.5Sc–0.3Zr alloy was processed by rolling, solution treatment and high-to-low two-step ageing. The microstructure contained thermally stable Al3(Sc,Zr) dispersoids and dense η′-MgZn2 precipitates with an equivalent diameter of 4.7 ± 2.0 nm. The Aged alloy achieved a 0.2% proof strength of 687 MPa, an ultimate tensile strength of 708 MPa and 8.8% elongation. Variant-resolved microscopy revealed four η′ orientations, localized interfacial strain and possible local stacking faults. Ageing increased the 0.2% proof strength by 56.8%, accompanied by greater strain localization and a transition towards mixed-mode fracture. This hierarchical architecture enables effective strengthening of conventionally processed high-Zn aluminium alloys.